Specifying Compression Gaskets for Structurally Glazed Curtain Walls
Structural glazing gets most of the attention in a façade specification, because the structural silicone bond is what holds a lite of glass to the frame of a 40-storey tower. The compression gasket hiding in the rebate rarely gets discussed until something goes wrong: a seal that has relaxed, a bond that has stained, or an edge of glass chipped on its way to site. Getting the gasket right is inexpensive compared with the cost of touching up a curtain wall, and on a tower in Melbourne or Sydney that cost includes crane time, access platforms and usually a night shift.
This article covers what a compression gasket does inside a structurally glazed frame, which elastomer compounds suit Australian conditions, how to set the compression range and tolerance stack out in the documentation, and what to check during installation and handover. It is written for developers, architects, main contractors and building owners in Australia who are assembling the envelope package and need enough detail to hold a supplier to the mark.
What the compression gasket does in the frame
In a structurally glazed system, the insulated glass unit is bonded to the aluminium frame rebate with a two-part structural silicone, and a gasket sits between the edge of the glass and the frame. As the lite is pushed home, the gasket is squeezed. That squeeze does three jobs at once: it seals the joint against air and dust, it absorbs the mismatch between glass size and frame opening, and it stops the glass edge working directly against aluminium as the frame moves under wind and temperature.
The distinction from conventional glazing matters. In a stick system, wedge or channel gaskets hold the glass in place and share the load. With structural silicone, the sealant carries the load and the gasket becomes a seal and a tolerance device. Because the gasket no longer props up the glass, its hardness and compression influence edge stress directly. A soft gasket can extrude into the structural silicone bead, while a hard one can chip the spacer or the edge of the unit.
It also keeps the seal line clean, which matters more in Australia than in a temperate European market. The gasket is not the drainage route. Frames still need internal weeps that discharge outside, and a gasket specified to the wrong width can close the slot the frame relies on. Specify the gasket profile against the frame extrusion rather than a generic catalogue drawing, and confirm the weep path with the façade consultant before the extrusion is ordered.
Elastomer compounds for Australian heat, UV and salt
Black EPDM is the workhorse for a reason. It is closed-cell, resists ozone and ultraviolet exposure, holds its compression set over a wide temperature range, and does not stain glass or coated aluminium. Fabricators typically use a 60 to 80 Shore A compound for curtain wall gaskets, and the exact durometer belongs in the specification rather than hiding behind the word "EPDM".
Silicone, or VMQ, is the alternative where temperature, movement or silicone-to-silicone contact demands it. Natural rubber and PVC-based gaskets tend to fail under UV and heat, and plasticisers in cheaper compounds can migrate into a structural silicone bond, which is why gasket and sealant need approving as a pair. Where an assembly sits in a bushfire-prone region such as Wagga Wagga, Bendigo or the Perth Hills, the polymer components in the glazing joint also need checking against AS 1537.4.
Local climate decides the rest. Darwin, Cairns and Townsville combine cyclonic wind loading under AS/NZS 1170.2 with salt-laden air, and coastal towers around the Gold Coast see persistent humidity. EPDM handles that, provided the stainless fixings and the frame coating are specified to match. In a Melbourne or Brisbane summer a west-facing dark lite can push the rebate past 70 degrees Celsius, so check the gasket's continuous working range against the actual surface temperature of the assembly, not the ambient design temperature.
Sizing, tolerances and the compression calculation
Gaskets are published with a compression figure, usually somewhere between 15 and 25 per cent for a closed-cell EPDM profile. The section is sized so that when the frame closes to its nominal rebate depth it is compressed by that amount, and the calculation has to survive every tolerance in the stack. A six millimetre free height closing to 4.8 millimetres gives 20 per cent compression; if closure varies across the building between 4.5 and 4.9 millimetres, the same gasket sits anywhere between 18 and 25 per cent.
That sensitivity is the point. Half a millimetre of variation in closure shifts compression by roughly eight percentage points, so closure tolerance, insulated glass unit manufacturing tolerance and frame deflection all need listing on the drawings. Slender sticks on a coastal tower can deflect several millimetres at the design wind pressure, and erection tolerance on a tall building in Sydney adds more. Specify gasket width, free height, material, durometer, the acceptable compression band and the maximum allowable stretch during installation.
Ask for independent verification where the tolerances are tight. An independent engineering review of the gasket specification, checked against the frame extrusion and the deflection figures, catches an arithmetic problem long before it becomes a procurement variation on site. It also gives the main contractor a defensible position when a supplier offers a cheaper profile with a similar material description.
Gaskets should be identifiable on site. Extrusions are commonly cut with a profile code or date stamp so an inspector can match what sits in the rebate to the approved detail, and the compound hardens with age, so ask for the date of manufacture and a maximum storage period. A gasket stretched over a sharp edge during glazing loses cross-section permanently and will sit under-compressed for the life of the building.
Sealant, setting blocks and neighbouring interfaces
The compression gasket does not work alone. The structural silicone is the primary seal and the structural element, and it has to be approved alongside the gasket compound so neither migrates into the other. Require the gasket supplier to confirm compatibility, and require the sealant to carry the usual classifications plus a peel adhesion test result, typically to ASTM C 794, on a full-size mock-up of the lite, the spacer and the rebate.
Setting blocks do the work the gasket does not. EPDM or silicone setting blocks sit in the base channel, sized to carry the weight of the unit with a few per cent of compression, with two blocks per lite at the quarter points and three for larger units. Specify them separately from the compression gasket, because a drawing showing one gasket profile in the base channel tends to leave the real compression gasket undefined.
Then there are the junctions. The seal line runs into spandrels, openings and the roof interface, and every break in that line is a detail somebody has to draw. Where a curtain wall lands beside a roof garden, a planter box or a green roof, the green roof interface checklist covers how those junctions are detailed so a planter upstand does not bridge the compressed seal or block the weeps. The same discipline applies where the glazing meets a Colorbond steel roof or a membrane podium on a mixed-use development.
Proving it on site and at handover
Quality assurance starts before the frame is closed. Ask for a water penetration test of the assembly against the relevant Australian Standard, a check of gasket compression on a trial assembly, and a sample of the installed gasket cross-section measured against the specified free height and durometer. On site, reject unlabelled or stretched gaskets, and reject any substituted profile that has not been approved in writing, since an unapproved substitution can void the structural silicone warranty.
The condition of the frame line matters too. Our guidance on site preparation after demolition covers how the working platform and frame line are protected once the old structure is gone, because plaster, dust and general site swarf will lodge in a gasket expected to seal for thirty years.
Handover documents should carry the compound type, durometer, compression range, batch and date marks, test reports, and a maintenance note warning against solvent cleaners that attack EPDM. The commercial structure of the Australian market decides who owns that paperwork. Under a supply-and-install package the fabricator carries it; on a supply-only package, common when a developer nominates a system and the builder buys it separately, the building owner should insist on the same records. In NSW, building work over $150,000 requires a Principal Contractor Award, and that holder carries site safety and quality duties, so the gasket inspection line has to be written into the contract rather than assumed. A change of compound that never reaches the drawings is a variation waiting for the quantity surveyor to price.